Super duplex 2507 vs Super duplex S32760

Super duplex 2507 (UNS S32750) vs Super duplex S32760 (UNS S32760): chemical composition and mechanical properties side by side.

PropertySuper duplex 2507Super duplex S32760
FamilySuper duplexSuper duplex
UNSS32750S32760
EN / W.Nr1.4410 X2CrNiMoN25-7-41.4501 X2CrNiMoCuWN25-7-4
Basis specASTM A240ASTM A240
Density g/cm³7.87.8
Chemical composition, %
C0.0300.030
Mn1.201.00
P0.0350.030
S0.0200.010
Si0.801.00
Cr24.0–26.024.0–26.0
Ni6.0–8.06.0–8.0
Mo3.0–5.03.0–4.0
N0.24–0.320.20–0.30
Cu0.500.50–1.00
W–0.50–1.00
Mechanical properties (min)
Tensile strength795 MPa (115 ksi)750 MPa (109 ksi)
Yield strength (0.2%)550 MPa (80 ksi)550 MPa (80 ksi)
Elongation15%25%
Hardness (max)310 HB270 HB
PREN (min, from spec)37.737.1

Single values are maximums; ranges are min–max; "bal" = balance. Limits are typical of the basis specification for that product form — forgings, pipe and fittings specifications differ slightly. Always check the exact specification, edition and the mill test certificate.

Compare with more grades →

Frequently asked questions

What is the difference between Super duplex 2507 and Super duplex S32760?

Strength: Super duplex S32760 minimum yield is 550 MPa vs 550 MPa for Super duplex 2507 (+0%); tensile 750 vs 795 MPa. Density: 7.8 vs 7.8 g/cm³ — same weight for the same dimensions. Pitting resistance (PREN, min): 37.7 vs 37.1 — higher for Super duplex 2507.

Which is stronger, Super duplex 2507 or Super duplex S32760?

Super duplex 2507 has the higher minimum yield strength (550 MPa vs 550 MPa).

Last updated 2026-11-02